MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco SUPREME Antifreeze/Coolant, Concentrate
Categories: Fluid

Material Notes: Features

Chevron SUPREME Antifreeze/Coolant is a superior quality, single phase, ethylene glycol based product blended with a premium quality additive package. It is a low silicate, all-purpose coolant designed for use in both heavy-duty diesel and automotive engines, particularly those containing aluminum alloys. Chevron SUPREME Antifreeze/Coolant is free of nitrites and amines.

Chevron SUPREME Antifreeze/Coolant provides antifoam properties, and rust and corrosion protection for aluminum, brass, copper, solder, steel and cast iron. It mixes readily with any clean tap water and is compatible with cooling system filters and supplemental additives.

Chevron SUPREME Prediluted 50/50 Antifreeze/Coolant is a 50/50 mixture of Chevron SUPREME Antifreeze/Coolant with deionized water.

Applications

Chevron SUPREME Antifreeze/Coolant is specially formulated to meet the stringent aluminum corrosion protection requirements of automotive engines. Because of its low concentration of silicate, it also complies with Cummins and other heavy-duty diesel engine manufacturers silicate requirements. This product is also suitable for use in industrial internal combustion engines where an antifreeze/coolant is required to provide protection against freezing, boil over, and corrosion.

Chevron SUPREME Antifreeze/Coolant does not meet DEX-COOL® requirements.

Note: These products are not to be used to protect the inside of potable water systems against freezing.

Key Words: CPS Number: 227800; MSDS Number: 10448
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/cc
pH 10.510.51:2 dilution with water; ASTM D1287
 
Thermal PropertiesMetricEnglishComments
Melting Point -34.0 °C-29.2 °F
 
Descriptive Properties
ColorFluorescent Green
Reserve Alkalinity ASTM D112112
Silicate, %0.09

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco DEX-COOL® Extended Life Antifreeze/Coolant, Prediluted 50/50
ChevronTexaco DEX-COOL® Extended Life Antifreeze/Coolant, Concentrate
ChevronTexaco Delo® Extended Life Coolant System, Coolant/Antifreeze
ExxonMobil Coolant/Antifreeze Mobil Heavy Duty
ExxonMobil Mobil Delvac Coolant/Antifreeze Extended Life 50/50 Prediluted

WCHEV421 / 75036

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.