MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chosun Refractories AC-1 Acid-Proof and Heat-Resistant Brick
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.20 g/cc0.0795 lb/in³
Water Absorption 0.30 %0.30 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 118 MPa17100 psiCold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.80 µm/m-°C
@Temperature 1000 °C
3.78 µin/in-°F
@Temperature 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 18 %18 %
Fe2O3 0.50 %0.50 %
SiO2 76 %76 %
 
Descriptive Properties
QualitiesAcid proof

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Esstech X-846-0000 Methacroyloxyethyl Maleate, C10H12O6
Celanese 50000873 Di-n-Butyl Maleate (DBM)
Zircar Ceramics AX-200 Refractory Supported Heater
TIMCAL ENSACO™ 150G Conductive Carbon Black
Celanese 50000433 Dioctyl Maleate (DOM)

CCHOS078 / 124022

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.