MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® MP-2951 XRD1 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene MP-2951 XRD1 is general purpose thermoplastic elastomer designed for a variety of consumer and industrial applications requiring a soft, rubber-like feel. Monprene MP-2817H is a low hardness, low density, RoHS compliant grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Filled; Good Flow; High Flow; Medium Density; High Hardness

Uses: Consumer Applications; Furniture; General Purpose; Grommets; Handles

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Viscosity 110 cP
@Shear Rate 206 1/s,
Temperature 200 °C
110 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  78
@Time 5.00 sec
78
@Time 0.00139 hour
Injection Molded; ASTM D2240
 80
@Time 1.00 sec
80
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 7.72 MPa1120 psiASTM D412
Tensile Stress at Strain 3.30 MPa
@Strain 100 %
479 psi
@Strain 100 %
ASTM D412
Elongation at Break 670 %670 %ASTM D412
Compression Set 64 %
@Temperature 70.0 °C,
Time 79200 sec
64 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 204 °C360 - 400 °F
Rear Barrel Temperature 182 - 204 °C360 - 400 °F
Middle Barrel Temperature 182 - 204 °C360 - 400 °F
Front Barrel Temperature 182 - 204 °C360 - 400 °F
Nozzle Temperature 182 - 204 °C360 - 400 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex MONPRENE® MP 2850E Thermoplastic Elastomer
Teknor Apex MONPRENE® MP 2850M Thermoplastic Elastomer

PTEKNQ0882 / 237373

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.