MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay SOPROPHOR® 3 D 33 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Soprophor® 3 D 33 is Tristyrylphenol Ethoxylate Phosphate Ester (acid form). It is multipurpose dispersing, wetting agent recommended for low pH formulations. It is excellent dispersant with unusual hydrophobe and compatibility with pigments.

Identification: ETHOXYLATED POLYARYLPHENOL PHOSPHATE ESTER

CAS: 90093 – 37 – 1

Solubility: Soluble in water and most polar and aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Agrochemical formulations : Dispersing, wetting and compatibility agent for SC formulation. Industrial formulations: Dispersant for industrial formulations. Polymer systems specialties: Excellent dispersant with unusual hydrophobe. Excellent compatibility with pigments.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³
pH 1.5 - 3.01.5 - 3.05% in water; RPG02
 
Thermal PropertiesMetricEnglishComments
Pour Point 0.000 °C32.0 °F
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 2.5 %<= 2.5 %RPG16
 
Descriptive Properties
AppearanceViscous yellow liquid
CompositionActive>97.5%
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay SOPROPHOR® 4 D 384 Surfactant
Solvay SOPROPHOR® BSU Surfactant
Solvay SOPROPHOR® CY/8 Surfactant
Solvay ANTAROX® PL 122 Surfactant
Solvay ANTAROX® B/848 Surfactant

WRHOD512 / 137743

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.