MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M FP083 Clear Polypropylene Label Products
Categories: Polymer; Adhesive

Material Notes: 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a high clarity general purpose acrylic emulsion that exhibits good initial tack, excellent die cutting properties, minimal cold flow, and good UV resistance.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milFacestock
 178 microns7.00 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.526 kN/m3.00 pli180° Peel, 12"/min., 1" wide sample; TLMI Method
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 5.00 °C>= 41.0 °FApplication
 <= 49.0 °C<= 120 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive TypeP1212 Perm18
Appearance78# CCK

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow H110-02N Polypropylene Homopolymer Resin
Vibrantz Technologies EG 2928 Glaze and Sealant Glass
Schott MEMpax® Borosilicate Glass
Schott Glass 8250 Borosilicate Glass
Eastman Eastar GN077 Copolyester, Natural

PMM33828 / 168575

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.