MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Extrusion 78761 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Note: NSF listings are obtained on specific colors.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 808015 sec; ASTM D2240
Tensile Strength, Yield 50.3 MPa7300 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.83 GPa410 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 2.90 GPa421 ksiASTM D790
Izod Impact, Notched  0.480 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.899 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
 0.530 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy  62.3 J/cm
@Temperature 23.0 °C
0.117 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 145 J/cm
@Temperature 23.0 °C
0.272 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C28.9 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
@Thickness 3.18 mm
158 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.91 mm
V-0
@Thickness 0.0752 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
Agency RatingsNSF 14
 NSF 61
 NSF Type I
Ease of SizingGood
FeaturesGood Chemical Resistance
FormsCube
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification12454ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesRods

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
3D Systems RenShape® SL 7820 Stereolithography Plastic
XG Sciences xGnP® Graphene Nanoplatelets
Geon® Performance Solutions Vinyl Fittings M1000 Polyvinyl Chloride, Rigid

PH0POL0160 / 144729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.