MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa JH720 G20 20% Glass Fiber Reinforced PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes:
    Features:
  • High mechanical strength
  • Good size stability
  • Low tendency to warp
  • Good surface
  • Suitable for exact molding

    Applications:
  • Imaging equipment shell
  • OA body frame
  • Electrical equipment
  • Computer plug parts
  • CD-ROM, DVD

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc
@Temperature 23.0 °C
1.33 g/cc
@Temperature 73.4 °F
ASTM D792
Filler Content 20 %20 %Glass Fiber
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
@Temperature 23.0 °C
0.0030 - 0.0040 in/in
@Temperature 73.4 °F
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8484ASTM D785
Tensile Strength at Break 97.0 MPa14100 psi10mm/min; ASTM D638
Elongation at Break 9.0 %9.0 %10mm/min; ASTM D638
Flexural Strength 140 MPa20300 psi2mm/min; ASTM D790
Flexural Modulus 6.20 GPa899 ksi2mm/min; ASTM D790
Izod Impact, Notched 1.35 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.53 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched 5.80 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
10.9 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohm1.00e+15 ohmASTM D257
Dielectric Strength 22.0 kV/mm559 kV/in1.6mm; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
@Thickness 6.40 mm
288 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
@Thickness 6.40 mm
280 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 295 °C<= 563 °F
Rear Barrel Temperature 240 - 270 °C464 - 518 °FStart Point: 260°C
Middle Barrel Temperature 250 - 280 °C482 - 536 °FStart Point: 265°C
Front Barrel Temperature 260 - 290 °C500 - 554 °FStart Point: 275°C
Melt Temperature 250 - 280 °C482 - 536 °FStart Point: 260°C
Mold Temperature 80.0 - 130 °C176 - 266 °FStart Point: 90°C
Drying Temperature 110 - 120 °C
@Time 10800 - 14400 sec
230 - 248 °F
@Time 3.00 - 4.00 hour
Pre-dry
Back Pressure 0.300 - 1.00 MPa43.5 - 145 psi
 
Descriptive Properties
Injection Speed60-90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BLUESTAR LXS 314 G30 PPE-HIPS, 30% Glass Filled
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Mitsubishi Iupilon® GSH 2020KR Polycarbonate
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
Kotec Carbotex KG-20MRA Polycarbonate, 20% Glass Fiber Reinforced

PKINGF044 / 104303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.