MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Honeywell A-C® 415 EVA copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Ethylene vinyl acetate (EVA) copolymer in prill form, with a VA content of 15%, developed specifically to be used as an adhesive flooding compound between the cable bundle and extruded outer jacket in the manufacturing of cables. Also can be used in candles and adhesives.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
Brookfield Viscosity 1300 cP
@Temperature 140 °C
1300 cP
@Temperature 284 °F
 
Thermal PropertiesMetricEnglishComments
Dropping Point 89.0 °C192 °FMettler
 
Descriptive Properties
Hardness12.5 dmmASTM D5
Product FormPrill

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell A-C® 400A EVA copolymer
Honeywell A-C® 405T EVA copolymer
Honeywell A-C® 645P EVA copolymer Oxidized
Honeywell A-C® 540 EVA copolymer
Honeywell A-C® 430 EVA copolymer

PHONWL028 / 179573

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.