MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Covestro Desmopan® 3059D Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; with release agent; excellent abrasion resistance; good wear resistance; very short cycle times; Application; Heel patches; Rollers; Boot shells; Injection molded engineering parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9797ISO 868
Hardness, Shore D 5959ISO 868
Tensile Strength, Ultimate 50.0 MPa7250 psi200 mm/min; b.o. ISO 527-1,-3
Tensile Stress at Strain  21.0 MPa
@Strain 100 %
3050 psi
@Strain 100 %
200 mm/min; b.o. ISO 527-1,-3
 42.0 MPa
@Strain 300 %
6090 psi
@Strain 300 %
200 mm/min; b.o. ISO 527-1,-3
Elongation at Break 400 %400 %200 mm/min; b.o. ISO 527-1,-3
Tensile Modulus  0.181 GPa
@Temperature 60.0 °C
26.3 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.586 GPa
@Temperature 20.0 °C
85.0 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 2.435 GPa
@Temperature -20.0 °C
353.2 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Flexural Modulus 0.180 GPa26.1 ksi2 mm/min; ISO 178
Rebound 35 %35 %Resilience; ISO 4662
Tear Strength 160 kN/m913 pli500 mm/min; ISO 34-1
Abrasion 1818mm³, Method A; ISO 4649
Compression Set  24 %
@Temperature 23.0 °C
24 %
@Temperature 73.4 °F
72 hr; ISO 815
 42 %
@Temperature 70.0 °C
42 %
@Temperature 158 °F
24 hr; ISO 815
 24 %
@Temperature 70.0 °C,
Time 86400 sec
24 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 240 °C428 - 464 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 3055D Polyurethane
Covestro Desmopan® 3072D Polyurethane
Kolon KOPEL® KP3372 General Purpose TPE Resin
Covestro Desmopan® 1080A Polyurethane
Covestro Desmopan® 1350D Polyurethane

PB09785 / 92625

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.