KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pumping through most injection molding systems.Features- Selective self adhesion
- Non adhesion to metals
- Insert-molding and co-injection molding available
Information Provided by Shin-Etsu Silicones of America, Inc. |
LSR, Liquid Silicone Rubber |