MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Conventus Polymers Duraflex COPE72D Polyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Duraflex COPE72D is a High Performance Copolyester Elastomer with a 72 Shore D hardness. It maintains outstanding mechanical strength and flexibility even at low temperatures. This product has outstanding weatherability, chemical resistance, and heat resistance. It is an excellent solution for applications that require performance beyond what olefinic elastomers can provide.

Information provided by Conventus Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccISO 1183
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Water Vapor Transmission 146 g/m²/day9.40 g/100 in²/dayASTM D372
Oxygen Transmission Rate 947 cc/m²/day61.0 cc/100 in²/dayASTM D1434
Linear Mold Shrinkage, Flow 0.016 - 0.019 cm/cm0.016 - 0.019 in/inASTM D955
Melt Flow 25 g/10 min
@Load 16.0 kg,
Temperature 240 °C
25 g/10 min
@Load 35.3 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 72
@Time 15.0 sec
72
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 48.0 MPa6960 psiASTM D638
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Elongation at Break 400 %400 %ASTM D638
Flexural Modulus 0.686 GPa99.5 ksiISO 178
Izod Impact, Notched  0.490 J/cm
@Thickness 6.40 mm,
Temperature -40.0 °C
0.918 ft-lb/in
@Thickness 0.252 in,
Temperature -40.0 °F
 1.37 J/cm
@Thickness 6.40 mm,
Temperature 20.0 °C
2.57 ft-lb/in
@Thickness 0.252 in,
Temperature 68.0 °F
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO179/1Ea
Coefficient of Friction >= 1.0>= 1.0ASTM D1894
Tear Strength 205 kN/m1170 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.0 kV/mm381 kV/inIEC 60243-1
Comparative Tracking Index >= 600 V>= 600 VIEC60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 219 °C426 °FISO 11357-1,-2,-3
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51nD; ASTM D542
Haze 1.0 %1.0 %ASTM D1003
Gloss 73 %73 %45°; ASTM D2457
Transmission, Visible 91 %91 %Regular; ASTM D1003
 94 %94 %Total; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Conventus Polymers Duraflex COPE82D Copolyester Elastomer
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer
Eastman Neostar FN005 Elastomer
Envalior Arnitel® EL250 TPC-ET, Injection Molding

PCONV945 / 233863

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.