MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a corona surface treatment for improved bonding to inks and adhesives. Standard thicknesses are 50 and 75 gauge, although other thicknesses may be available upon special request. The treated side of P25T normally is wound toward the core, but this can be reversed upon request.

General Product Info: The 50 gauge film can be formed to a maximum draw depth of 1 1/8 in (28 mm), where the draw ratio (area/area) does not exceed 2.0. The 75 gauge P25T can be thermoformed to a maximum draw depth of 1 1/2 in (38 mm) with a maximum draw ratio of 2.25. Good temperature control is essential for satisfactory thermoforming. Observation of excessive web thinning and/or frequent "poppers" during thermoforming usually indicate that the forming temperature should be increased. The preferred process for making multilayered structures with P25T is through adhesive lamination, because relatively low web temperatures can be used. While extrusion coating also is an option, extra care must be taken to prevent unwanted stretching of the web. For the same reasons, care must be exercised when subjecting P25T to any converting process involving heating or drying.

Combinations of P25T and a sealant layer are used in peelable lidding, medical packaging, and as the formed web in hermetically sealed pouches for "heat-in-bag" applications for frozen entrees and vegetables. It is also used in similar applications, particularly where the oxygen barrier properties provided by PVdC-coated films are not required.

Approvals: FDA Food Contact Status - All gauges of Mylar® P25T comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® P25T can be used to contain foods during oven cooking or oven baking at temperatures above 250°F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Water Vapor Transmission 43.5 g/m²/day
@Temperature 38.0 °C
2.80 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249
Thickness 12.7 microns0.500 mil
Coating Weight 17.3 g/m²10.8 lb/ream0.5 m2; ASTM E252
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 170 %170 %ASTM D882A
Film Elongation at Break, TD 135 %135 %ASTM D882A
Secant Modulus, MD 2.96 GPa430 ksiASTM D882
Secant Modulus, TD 3.17 GPa460 ksiASTM D882
Coefficient of Friction, Static 0.500.50ASTM D1894
Graves Tear Strength 0.123 kN/m0.700 pliASTM D1004
Film Tensile Strength at Break, MD 152 MPa22000 psiASTM D882A
Film Tensile Strength at Break, TD 179 MPa26000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Maximum Service Temperature, Air 121 °C250 °F
Shrinkage, MD 2.8 %
@Temperature 150 °C,
Time 1800 sec
2.8 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 2.5 %
@Temperature 150 °C,
Time 1800 sec
2.5 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %5.0 %ASTM D1003
Gloss 120 %120 %20°; ASTM D2457
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Clarity71 percentASTM D1746
Gas Permeability (Base film)9 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)40100 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® RSX Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® RB43 Polyester Film, 100 Gauge

PDTZ9394 / 139714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.