Multi-Pro 4002 T H is a talc reinforced polypropylene compound with excellent stiffness at medium impact resistance. Its heat resistance is improved over natural and can resist 150°C for 750 hours in an accelerated oven aging test. This product meets CMP PP 010 specifications. Data provided by Multibase. |