MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned)  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Key Features:
  • Unfilled
  • High impact or high impact modified
  • Light stabilized or stable to light
  • Heat stabilized or stable to heat

Suitable processing methods:

  • Injection molding

Triax® is now a INEOS Styrolution trade name; this grade is discontinued. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³(DAM)
Melt Density 0.900 g/cc
@Temperature 260 °C
0.0325 lb/in³
@Temperature 500 °F
Water Absorption 6.0 %6.0 %(from DAM)
Moisture Absorption at Equilibrium 1.7 %1.7 %23°C/50% R.H. (from DAM)
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psi
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 13 %13 %
Tensile Modulus 1.05 GPa152 ksi
Charpy Impact Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Charpy Impact, Notched 7.40 J/cm²35.2 ft-lb/in²
 1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
Puncture Energy 38.0 J28.0 ft-lbPuncture energy +23°C
 40.0 J29.5 ft-lbPuncture energy -30°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cm
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
 6.7
@Frequency 100 Hz
6.7
@Frequency 100 Hz
Dielectric Strength 34.0 kV/mm864 kV/in
Dissipation Factor  0.055
@Frequency 1e+6 Hz
0.055
@Frequency 1e+6 Hz
 0.10
@Frequency 100 Hz
0.10
@Frequency 100 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 105 µm/m-°C
@Temperature 20.0 °C
58.3 µin/in-°F
@Temperature 68.0 °F
DAM
CTE, linear, Transverse to Flow 115 µm/m-°C
@Temperature 20.0 °C
63.9 µin/in-°F
@Temperature 68.0 °F
DAM
Specific Heat Capacity 2.20 J/g-°C0.526 BTU/lb-°FMelt
Thermal Conductivity 0.145 W/m-K1.01 BTU-in/hr-ft²-°FMelt
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °F(from DAM)
Vicat Softening Point 102 °C216 °F50°C/h 50N (from DAM)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding
Mold Temperature 80.0 °C176 °FInjection Molding
Ejection Temperature 90.0 °C194 °F
Injection Velocity 40.0 mm/sec1.57 in/sec
 
Descriptive Properties
Effective thermal diffusivity0.732E-7 m²/sMelt

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM)
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Ineos ABS Triax® 1180 ABS + Polyamide Blend (Conditioned)
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
INEOS Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned)

PB10339 / 26377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.