MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • Strong flexible bonds
  • Medium viscosity grade adhesive for many brush or flow applications
  • Quick drying
  • Excellent resistance to many fuels and oils
  • Bond leather, nitrile rubber, most plastics, gasketing materials to a variety of substrates
  • May be heat cured to obtain improved physical properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 22 - 26 %22 - 26 %
pH 4.1 - 4.54.1 - 4.5
Brookfield Viscosity 175 - 350 cP175 - 350 cPRVF #2 sp @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  0.0621 MPa
@Temperature 82.0 °C
9.00 psi
@Temperature 180 °F
Overlap, 1/8" Birch/Birch
 0.138 MPa
@Temperature 66.0 °C
20.0 psi
@Temperature 151 °F
Overlap, 1/8" Birch/Birch
 1.05 MPa
@Temperature 1.00 °C
152 psi
@Temperature 33.8 °F
Overlap, 1/8" Birch/Birch
 1.38 MPa
@Temperature 14.0 °C
200 psi
@Temperature 57.2 °F
Overlap, 1/8" Birch/Birch
Peel Strength  0.701 kN/m
@Temperature 14.0 °C,
Time 1.81e+6 sec
4.00 pli
@Temperature 57.2 °F,
Time 504 hour
180°, Canvas/Steel
 1.58 kN/m
@Temperature 82.0 °C,
Time 1.81e+6 sec
9.00 pli
@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
 2.28 kN/m
@Temperature 14.0 °C,
Time 86400 sec
13.0 pli
@Temperature 57.2 °F,
Time 24.0 hour
180°, Canvas/Steel
 2.80 kN/m
@Temperature 66.0 °C,
Time 1.81e+6 sec
16.0 pli
@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
 3.51 kN/m
@Temperature 1.00 °C,
Time 1.81e+6 sec
20.0 pli
@Temperature 33.8 °F,
Time 504 hour
180°, Canvas/Steel
 4.12 kN/m
@Temperature 14.0 °C,
Time 259000 sec
23.5 pli
@Temperature 57.2 °F,
Time 72.0 hour
180°, Canvas/Steel
 4.82 kN/m
@Temperature 14.0 °C,
Time 432000 sec
27.5 pli
@Temperature 57.2 °F,
Time 120 hour
180°, Canvas/Steel
 5.43 kN/m
@Temperature 14.0 °C,
Time 605000 sec
31.0 pli
@Temperature 57.2 °F,
Time 168 hour
180°, Canvas/Steel
 6.14 kN/m
@Temperature 14.0 °C,
Time 1.21e+6 sec
35.0 pli
@Temperature 57.2 °F,
Time 336 hour
180°, Canvas/Steel
 
Thermal PropertiesMetricEnglishComments
Flash Point -18.0 °C-0.400 °FCC
 
Descriptive Properties
AppearanceBrown
BaseNitrile Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive
3M Scotch-Grip™ 847 Rubber and Gasket Adhesive 847

PMM34120 / 168867

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.