MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nickel (II) Sulfide, NiS (Millerite)
Categories: Ceramic; Sulfide/Chalcogenide

Material Notes: Yellow hexagonal crystals

Key Words: Nickel Sulfide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.50 g/cc0.199 lb/in³
a Lattice Constant 9.616 Å9.616 Å
c Lattice Constant 3.152 Å3.152 Å
Formula Units/Cell (Z) 99
Molecular Weight 90.759 g/mol90.759 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 3.33.3
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility 0.000190.00019cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 331.6 J/g142.7 BTU/lb
Melting Point 976 °C1790 °F
 
Descriptive Properties
CAS Number16812-54-7
ColorYellow
Crystal StructureHexagonal - Rhombohedral

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Neodymium Telluride, Nd2Te3
Neodymium Sulfide, Nd2S3
Molybdenum (IV) Telluride, MoTe2
Molybdenum (IV) Sulfide, MoS2 (Molybdenite)
Molybdenum (IV) Selenide, MoSe2

EINOR0521 / 3650

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.