MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik CHROMA-CHEM® 844-1852 Industrial Colorant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CHROMA-CHEM 844 Colorants are designed specifically for use in high performance, non-aqueous, industrial and maintenance coatings. The various pigments utilized in this colorant line are dispersed in a proprietary acrylic resin vehicle. This vehicle provides excellent wetting and dispersing properties superior to other acrylic resins available.

The solvents used are a variable blend of Propylene Glycol Monomethyl Ether Acetate (PMA) and Naphthol Spirits. They are non-red label and conform to Rule 66 and similar regulations. Each colorant contains a carefully selected and unique blend of vehicle, solvent, pigment and surfactants to yield acceptance in a wide range of nonaqueous coatings applications. The individual CHROMA-CHEM 844 Colorant formulations are designed to minimize the surfactant and additive levels needed to achieve colorant acceptance in a variety of coatings systems.

The pigments in the CHROMA-CHEM were chosen to provide a wide range of hues and good durability, lightfastness and chemical resistance. However, the lightfastness and weathering properties of pigments depend a great deal on the coating in which they are used. Colorants should be tested under accelerated and actual weathering conditions to verify lightfastness and durability and to determine suitability for the desired use.

51274-00-1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Solids Content 30 %30 %pigment
 32.6 %32.6 %vehicle
Volatile Organic Compounds (VOC) Content 462 g/l462 g/l
Volatiles 37.4 %37.4 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
 
Descriptive Properties
Bleeding in LacquerNone
Bleeding in Linseed OilNone
Bleeding in Mineral SpiritsNone
Bleeding in ToluolNone
Color NameY-42
ColorantTrans Yellow Oxide
Light Fastness MassExcellent
Light Fastness TintExcellent
PigmentBASF L 1915
Resistance to Acids MassExcellent
Resistance to Acids TintExcellent
Resistance to Alkali MassExcellent
Resistance to Alkali TintExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik CHROMA-CHEM® 844-1054 Industrial Colorant
Evonik CHROMA-CHEM® 844-1063 Industrial Colorant
Evonik CHROMA-CHEM® 844-0453 Industrial Colorant
Evonik CHROMA-CHEM® 844-0451 Industrial Colorant
Evonik CHROMA-CHEM® 844-0353 Industrial Colorant

PHUMB140 / 81142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.