MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Data provided by the manufacturer.

Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In addition to standard molding and extrusion, Hylar® polymers lend themselves well to solution-applied coatings.

Key Words: Polyvinylidinefluoride; Polyvinylidine Fluoride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 - 1.77 g/cc0.0632 - 0.0639 lb/in³ASTM D792
Water Absorption 0.040 %0.040 %ASTM D570
Linear Mold Shrinkage 0.025 - 0.030 cm/cm0.025 - 0.030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 74 - 8074 - 80ASTM D2240
Tensile Strength, Ultimate 31.0 - 41.0 MPa4500 - 5950 psiASTM D638
Tensile Strength, Yield 28.0 - 41.0 MPa4060 - 5950 psiASTM D638
Elongation at Break 50 - 250 %50 - 250 %ASTM D638
Elongation at Yield 10 %10 %ASTM D638
Tensile Modulus 1.03 - 1.38 GPa149 - 200 ksiASTM D638
Flexural Yield Strength 45.0 - 52.0 MPa6530 - 7540 psiASTM D790
Flexural Modulus 1.138 - 1.793 GPa165.1 - 260.1 ksiASTM D790
Izod Impact, Notched 1.06 - 2.12 J/cm1.99 - 3.97 ft-lb/in
Izod Impact, Unnotched 8.00 - 20.0 J/cm15.0 - 37.5 ft-lb/inLow Temp; ASTM D256
Coefficient of Friction, Dynamic 0.10 - 0.250.10 - 0.25ASTM D1894
Coefficient of Friction, Static 0.14 - 0.200.14 - 0.20ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.10e+15 ohm-cm1.10e+15 ohm-cmASTM D257
Dielectric Constant  6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
ASTM D150
 7.2
@Frequency 60 Hz
7.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 10.4 kV/mm
@Thickness 3.20 mm
264 kV/in
@Thickness 0.126 in
Short-Time 500 V/sec
Dissipation Factor  0.030
@Frequency 60 Hz
0.030
@Frequency 60 Hz
ASTM D150
 0.16
@Frequency 1e+6 Hz
0.16
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 50 sec>= 50 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 140 µm/m-°C
@Temperature 20.0 °C
44.4 - 77.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.30 - 1.50 J/g-°C0.311 - 0.359 BTU/lb-°FDSC
Thermal Conductivity 0.190 - 0.220 W/m-K1.32 - 1.53 BTU-in/hr-ft²-°FASTM C177
Melting Point 160 °C320 °FASTM D3418
Maximum Service Temperature, Air 150 °C302 °FNo oxidative or thermal degradation after 5 years at 150°C (300°F)
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 90.0 °C176 - 194 °FTMA
Brittleness Temperature <= -62.0 °C<= -79.6 °FASTM D2236
Flammability, UL94 V-0V-0
Oxygen Index 43 %43 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.421.42
 
Processing PropertiesMetricEnglishComments
Processing Temperature 215 - 232 °C419 - 450 °FPreheat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMD Performance Livilux™ PDY-132 PPV copolymer
Arkema Kynar Flex® 3030-10 PVDF
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
3M Dyneon™ PVDF 60512/0000 Polyvinylidene Fluoride
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation

PTVFA1 / 71557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.