MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This phosphorus flame retardant grade, offers excellent filling qualities and with good mechanical properties. This grade is stabilized to offer a very low migration and corrosion of metallic contacts. It is particularly suitable for molding insulating parts for electrical devices: connectors, contactors, bobbins coil formers and thin parts under stress. This product is available in natural and black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183/A
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
0.90 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiISO 527 Type 1A
Elongation at Break 2.7 %2.7 %ISO 527 Type 1A
Tensile Modulus 8.70 GPa1260 ksiISO 527 Type 1A
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 7.90 GPa1150 ksiISO 178
Charpy Impact Unnotched 6.10 J/cm²29.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 V500 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75/Af
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
1210
Oxygen Index 28 %28 %ISO 4589
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3X2G5 BK23187 25% Glass Filled PA66 (Dry)
BASF Ultramid® A3UG5 BK 23260 25% Glass Filled PA66 (Dry)
Asia International Enterprise (Hong Kong) 60G5F Nylon 66, 25% Filled
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled
Eurotec® Tecomid® NA40 GR25 GR003 XA70 PA6.6, 25% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035

PRHOD729 / 137960

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.