MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE; Polypropylene (PP)

Material Notes: Product Description: Exxelor PO 1020 polymer resin is a high performance maleic anhydride fuctionalized homopolypropylene produced by reactive extrusion. It has been primarily designed to add polarity to polypropylene matrices and in particular improved polypropylene reactivity and amio-silane treated glass reinforcements. Its high content of maleic anhydride allows its use at low treat levels while maintaining optimum application properties.This grade is designed to:
  • Function as a coupling agent between reinforcing materials, such as glass fibers and inorganic fillers, and polypropylene.
  • Achieve compatibility in polypropylene/polyamide alloys.
  • Achieve compatibility between polyolefins and more polar polymers that are capable of interaction with maleic anhydride for alloying recycling or co-extrusion purpose.
  • Improve polypropylene-to-metal adhesion properties.

Key Features: Performance enhancements in glass-filled polypropylene:

  • Improved cost/performance balance compared to earlier generation modifiers
  • Easy molding of highly glass-filled compounds and/or comples and thin parts due to its high flow peroperties.
  • Outstandign unnotched Izod and Charpy performance
  • Excellent notched Izod and Charpy impact resistance
  • Improved tensile and flexural strength
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow  110 g/10 min
@Load 1.20 kg,
Temperature 190 °C
110 g/10 min
@Load 2.65 lb,
Temperature 374 °F
ASTM D1238
 430 g/10 min
@Load 2.16 kg,
Temperature 190 °C
430 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Collected Volatile Condensable Material <= 0.30 %<= 0.30 %AM-S 350.03
 
Thermal PropertiesMetricEnglishComments
Melting Point 162 °C324 °FPeak; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Yellow Index <= 30 %<= 30 %ASTM E313-96
 
Descriptive Properties
Maleic anhydride graft levelhighFTIR EPK-04 QT-02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene
Dow Engage® 8400 Polyolefin Elastomer
Dow Engage® 8411 Polyolefin Elastomer
BYK PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin

PEXB513 / 37818

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.