MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem® Guard 349 Nonionic, polyethylene dispersion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Nonionic, polyethylene dispersion

Usage: Michem® Guard 349 is designed to impart rub resistance, block resistance and matting properties to aqueous paints, coatings and inks.

Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooring

Food Contact Information when manufactured in Belgium:
FDA:
175.300: Resinous and polymeric components of coatings. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 - 0.980 g/cc0.960 - 0.980 g/cc
Volatiles 49.5 - 50.5 %49.5 - 50.5 %
pH >= 7.0>= 7.0Recommended pH of system
 6.5 - 8.56.5 - 8.5
Brookfield Viscosity 500 - 1000 cP500 - 1000 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceWhite liquid
Emulsifier ChargeNonionic
Solids TypePolyethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Michem® Tite 242AF Skin packaging primer
Momentive Performance Materials AC6091 Boron Nitride (BN) Powder
Michelman® Michem® Tite 335AF Skin packing / heat seal coating

WMICHEL129 / 135046

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.