MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolene® E6210C High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Formolene® E6210C is a bimodal high molecular weight high density resin pressure pipe resin. It contains an enhanced additive package for increased oxidative resistance in potable water systems.

When blended with the approved color concentrate, Formolene® E6210C complies with the following industry standards:
Cell Classification: 445574C CC2 per ASTM D3350
Material Rating Designation for E6210C - Per ASTM a PE 4710 resin with an HDB of 1,600 psi@73ºF and 1,000 psi @ 140ºF per PPI TR-4 - Per ISO a PE 100 resin with an MRS 10 at 20ºC. It meets the requirements for a PE 100 compound as qualified by ISO 9080 and ISO 12162
Meets NSF 14 and 61 for use with potable water systems

Suggested Applications: Potable Water; Oil and Gas Gathering and Distribution; Chemical, Industrial and Mining; Sewer Systems.

Information provided by Formosa Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³Natural; ASTM D1505
 0.957 g/cc0.0346 lb/in³Pigmented Black (4.5% letdown); ASTM D1505
Melt Flow  0.040 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.040 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 6.7 g/10 min
@Load 21.6 kg,
Temperature 190 °C
6.7 g/10 min
@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 2000 hour>= 2000 hourASTM F1473
Tensile Strength, Yield >= 24.1 MPa>= 3500 psi2 in/min, Type IV bar; ASTM D 638
Elongation at Break >= 600 %>= 600 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus >= 0.793 GPa>= 115 ksi2% secant, (16:1 span:depth, 0.5 in./min.); ASTM D790
Flexural Modulus, 1% Secant >= 931 MPa>= 135000 psi16:1 span:depth, 0.5 in./min.; ASTM D790
Izod Impact, Notched 4.86 J/cm
@Thickness 3.17 mm
9.10 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -70.6 °C<= -95.0 °FType A, Type I specimen; ASTM D746
 
Descriptive Properties
Thermal Stability Temperature>500 °FASTM D3350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® HP4525 High Density Polyethylene
Formosa Plastics Formolene® HB6007F High Density Polyethylene
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE
Formosa Plastics Formolene® E6210A High Density Polyethylene
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene

PFPCPQ9004 / 239825

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.