MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ THV 610GZ Fluoroplastic Granules  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: 3M™ Dyneon™ Fluoroplastic Granules THV 610GZ provides a balance of low permeation, thermal stability, and melt processability. It can be used to prepare molded parts and extruded films, tubes, profiles and wire coatings. It is useful for applications that require flexibility and good chemical resistance. This product processes at higher temperatures than that of 3M THV grades; therefore, the use of corrosion - resistant equipment is suggested.

Features and Benefits:

  • Excellent flexibility
  • Higher transparency
  • Excellent chemical permeation resistance
  • Bondable to itself and other substrates (for multi-layer constructions)
  • Processing profile allows co-processing with other plastics and hydrocarbon elastomers

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.04 g/cc2.04 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 265 °C
10 g/10 min
@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Flexural Modulus 0.490 GPa71.1 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 185 °C365 °FASTM D4591

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ THV 221GZ Fluoroplastic Granules
3M Dyneon™ THV™ 200P Fluorothermoplastic, Powder Form
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate
3M Dyneon™ THV 220G Fluorothermoplastic
3M Dyneon™ THV™ 500 Fluorothermoplastic

PDYL9960 / 129978

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.