MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips MC3200 Crystal Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: High heat crystal polystyrene.

Applications:

  • Medical parts
  • Consumer containers, vials, jars, etc.
  • Clock lenses
  • Audio cassettes
Features:
  • Fast cycling due to high heat distortion
  • High Vicat softening temperature
  • Excellent clarity
  • Balanced flow - heat distortion characteristics

Information provided by Chevron Phillips

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D-792
Bulk Density 0.609 - 0.673 g/cc0.0220 - 0.0243 lb/in³
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/in24 hours; ASTM D-955
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.0 MPa7400 psi0.2 in/min; 0.125" thickness; ASTM D-638
Elongation at Yield 4.5 %4.5 %0.2 in/min; 0.125" thickness; ASTM D-638
Tensile Modulus 3.10 GPa450 ksi0.2 in/min; 0.125" thickness; ASTM D-638
Flexural Strength 69.0 MPa10000 psi0.1 in/min; 0.250" thickness; ASTM D-790B
Flexural Modulus 3.10 GPa450 ksi0.1 in/min; 0.250" thickness; ASTM D-790B
Izod Impact, Notched 0.190 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
0.356 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 6.35 mm
194 °F
@Thickness 0.250 in
ASTM D-648
Vicat Softening Point 107 °C
@Thickness 6.35 mm
225 °F
@Thickness 0.250 in
Rate B; ASTM D-1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips MC3650 Crystal Polystyrene
Chevron Phillips EA3350 Crystal Polystyrene
Chevron Phillips EA3025 Crystal Polystyrene
Videolar-Innova 535 Crystal Polystyrene (GPPS)
Network Polymers 702 Polystyrene

PCHEVD266 / 20760

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.