MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES HiFill® PP 0096 S LE Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Unspecified Filler/Reinfor

Features: Low Extractables

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm
@Thickness 3.17 mm
0.019 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 33.1 MPa4800 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Strength 35.9 MPa5200 psiASTM D790
Flexural Modulus 1.31 GPa190 ksiASTM D790
Izod Impact, Notched 0.267 J/cm
@Thickness 3.17 mm
0.500 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 34.2 µm/m-°C19.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 116 °C240 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® ABS GF5 5% Glass Filled
Techmer ES HiFill® PP GF10 10% Glass Filled
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled
Techmer ES HiFill® ABS 1067
Techmer ES HiFill® ABS 0350

PTPC0531 / 136469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.