MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 204°C Temper
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainless steels. Oil quenching this alloy from temperatures between 1800°F and 1950°F produces the high strength and/or wear resistance as well as corrosion resistance.

A major use for this grade of heat treatable stainless steel is in cutlery. When blanking cutlery parts from annealed raw material stock, Type 425 Mod will usually exhibit hardness, yield strength, and tensile strength that are low enough for fine blanking purposes.

UTS, TYS, and hardness values below obtained after austenitizing at 1800-1950°F (982-1066°C) followed by an oil quench and two hour temper.

Information provided by Allegheny Ludlum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.72 g/cc0.279 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5353
Tensile Strength, Ultimate 1868 MPa270900 psiTypical
Tensile Strength, Yield 1385 MPa
@Strain 0.2 %
200900 psi
@Strain 0.2 %
typical
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000610 ohm-cm0.0000610 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.6 µm/m-°C
@Temperature 20.0 - 200 °C
6.44 µin/in-°F
@Temperature 68.0 - 392 °F
 12.8 µm/m-°C
@Temperature 20.0 - 600 °C
7.11 µin/in-°F
@Temperature 68.0 - 1110 °F
Thermal Conductivity 24.207 W/m-K
@Temperature 100 °C
168.00 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 1472 - 1510 °C2682 - 2750 °F
Solidus 1472 °C2682 °F
Liquidus 1510 °C2750 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 - 0.55 %0.50 - 0.55 %
Chromium, Cr 13 - 14 %13 - 14 %
Iron, Fe 85 %85 %as balance
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 0.80 - 1.2 %0.80 - 1.2 %
Nickel, Ni <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AIM 47 Fusible Bismuth Alloy
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 204°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper

NL4251 / 17927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.