MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omni Plastics OmniCarb™ PC GR10 Polycarbonate, 10% Glass Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: 10% Glass Reinforced; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Filler Content 10 %10 %ASTM D2584
Melt Flow 14 g/10 min14 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 2.965 GPa430.0 ksiASTM D790
Izod Impact, Notched 1.71 J/cm
@Thickness 3.17 mm
3.20 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 3.17 mm
280 °F
@Thickness 0.125 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
@Thickness 3.17 mm
275 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Omni Internal Testing
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 293 °C480 - 560 °F
Middle Barrel Temperature 271 - 304 °C520 - 580 °F
Front Barrel Temperature 271 - 304 °C520 - 580 °F
Nozzle Temperature 271 - 304 °C520 - 580 °F
Melt Temperature 271 - 304 °C520 - 580 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Edinburg Plastics CBI625 PC/PBT, 10% Glass Filled
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
Covestro Makrolon® RW 2407 Polycarbonate
Covestro Makrolon® RW 2405 Polycarbonate, 10% Glass Fiber
Covestro Makrolon® GF9002 Polycarbonate, 10% Glass Filled

POMNI5119 / 185265

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.