MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

STAR Thermoplastic Alloys & Rubbers StarMediflex P 7020-1000 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Product Description: StarMediflex P 7020-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications.

Features:
Soft Touch
Rubbery Feel
Excellent Colorability

Processing Method: Injection Molding

Information Provided by STAR Thermoplastic Elastomers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Viscosity 4000 cP
@Shear Rate 10994 1/s,
Temperature 210 °C
4000 cP
@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 20
@Time 10.0 sec
20
@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 1.88 MPa
@Time 7200 sec
273 psi
@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 931 %
@Time 7200 sec
931 %
@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.379 MPa
@Time 7200 sec,
Strain 300 %
55.0 psi
@Time 2.00 hour,
Strain 300 %
Die C; ASTM D412
Tear Strength 8.41 kN/m48.0 pliASTM D624
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-105 Thermoplastic Elastomer
Polymax® Maxelast® P3915T TPE, PP Overmold or Standalone use
Polymax® Maxelast® P3816 TPE, PP Overmold or Standalone use
Teknor Apex Monprene® MP-2820M Thermoplastic Elastomer
Top Polymer Topolymer® 8218-P TPE

PSTAQ961 / 131270

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.