MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric
Categories: Metal; Nonferrous Metal; Copper Alloy; Nickel Alloy; Polymer; Thermoplastic; Nylon (Polyamide PA); Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave and meets UL94 flame class V0 reference E255577. NF32B050A21 can be supplied with self-adhesive backing, temperature melt adhesive or no adhesive

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 100 - 140 microns3.94 - 5.51 mil
 
Mechanical PropertiesMetricEnglishComments
Abrasion 500000500000[cycles]; ASTM D4966
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.050 ohm<= 0.050 ohmASTM F390
Shielding Effectiveness  68 dB
@Frequency 3.00e+9 Hz
68 dB
@Frequency 3.00e+9 Hz
ASTM D4935-99
 82 dB
@Frequency 1e+7 Hz
82 dB
@Frequency 1e+7 Hz
ASTM D4935-99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
P & P Technology M W Conductive Fabric
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket
P & P Technology MW Series Conductive Fabric
Parker Chomerics SOFT-SHIELD® 3700 High Temperature Conductive Fabric Over Foam
Constantan Thermocouple Wire

PPPTEC004 / 133468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.