MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram Metal Cap PL380Z81 Heavy Density Polyethylene, 81% Mineral Filled
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: 81% Mineral filled, heavy density polyethylene for injection molding metalized part and galvanized covers.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.00 g/cc0.108 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inISO 2577
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram RamOfin PPC370B73 Polypropylene, 73% Mineral Filled
Polyram Metal Cap PPC373B72 Polypropylene, 72% mineral Filled
Polykemi AB POLYfill PPH BF4075 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Polykemi AB POLYfill PPH B8075 Polypropylene Homopolymer, Mineral Reinforced
Polykemi AB POLYfill PPC B8075 Polypropylene Copolymer, Mineral Reinforced

PPOLYR977 / 126774

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.