MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Sapphire 5.0 Ink Primer
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Primer for use with HP Indigo press.

Q4310A (Sapphire 5.0) is designed as a primer for HP Indigo substrates to render them compatible to ink. It can be used on paper substrates.

Q4310A (Sapphire 5.0) can be applied via flexo or direct gravure systems. The recommended dry coat weight is 30 to 60 mg/m². Use our Sapphire Indicator Solution to check quality of the coating. The anilox should be kept turning at all times to avoid premature drying of the solution. Cleaning with warm water, IPA or slightly acidic water is recommended.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 1.02 g/cc0.980 - 1.02 g/cc
Volatiles 94.75 - 95.25 %94.75 - 95.25 %
pH <= 11<= 11
Brookfield Viscosity 30 - 35 cP30 - 35 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceTranslucent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Mateck Sapphire (Al2O3)
Schott Sapphire Optical Window
Zinc Selenide, ZnSe
Zinc Sulfide, ZnS, Wurtzite

WMICHEL190 / 135107

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.