MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Vinyl (PVC)

Material Notes:
Material Status-Commercial: Active
Availability-North America
Test Standards Available-ASTM
Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather Resistance
Uses- Footwear, Tubing, Gaskets, Weatherstripping, hose, Wheels, Seals
Forms-Pellets
Processing-Extrusion, Injection Molding

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Linear Mold Shrinkage 0.010 - 0.025 cm/cm0.010 - 0.025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 454515 seconds; ASTM D2240
Tensile Strength, Yield 2.55 MPa370 psi100%; ASTM D412
 8.62 MPa1250 psiASTM D412
Elongation at Break 390 %390 %ASTM D412
Tear Strength 22.8 kN/m130 pliDie C; ASTM D624
Compression Set  23 %
@Temperature 22.8 °C,
Time 79200 sec
23 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 57 %
@Temperature 70.0 °C,
Time 79200 sec
57 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -56.1 °C-69.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 350 °F
Middle Barrel Temperature 160 - 177 °C320 - 350 °F
Front Barrel Temperature 160 - 177 °C320 - 350 °F
Mold Temperature 23.9 - 51.7 °C75.0 - 125 °F
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
 
Descriptive Properties
Screw Compression Ratio2:1-3:1
Screw L/D Ratio20:1- 24:1
Suggested Max Regrind, %20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer
Teknor Apex Flexalloy® 3500-70 Polyvinyl Chloride Elastomer

PTEKNO163 / 69906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.