MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Arnitel® EM460 TPC-ET, Injection Molding or Extrusion Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Injection Molding or Extrusion Grade

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption 0.70 %0.70 %Sim. ISO 62
Moisture Absorption 0.300 %0.300 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inSim. to ISO 294-4
Linear Mold Shrinkage, Transverse 0.0125 cm/cm0.0125 in/inSim. to ISO 294-4
Melt Flow 46 g/10 min
@Load 2.16 kg,
Temperature 230 °C
46 g/10 min
@Load 4.76 lb,
Temperature 446 °F
MVR, [cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 40
@Time 3.00 sec
40
@Time 0.000833 hour
ISO 868
Tensile Strength at Break 23.0 MPa3340 psiISO 527-1/-2
Tensile Stress at Strain  3.90 MPa
@Strain 5.0 %
566 psi
@Strain 5.0 %
ISO 527-1/-2
 6.60 MPa
@Strain 10 %
957 psi
@Strain 10 %
ISO 527-1/-2
 9.20 MPa
@Strain 50 %
1330 psi
@Strain 50 %
ISO 527-1/-2
 9.30 MPa
@Strain 100 %
1350 psi
@Strain 100 %
ISO 527-1/-2
Elongation at Break 800 %800 %Nominal; ISO 527-1/-2
Tensile Modulus 0.0850 GPa12.3 ksiISO 527-1/-2
Izod Impact, Notched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Dielectric Constant 4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
Dissipation Factor 0.035
@Frequency 1e+6 Hz
0.035
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 160 µm/m-°C88.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C88.9 µin/in-°FISO 11359-1/-2
Melting Point 189 °C372 °F10°C/min; ISO 11357-1/-3
Vicat Softening Point 50.0 °C
@Load 5.10 kg
122 °F
@Load 11.2 lb
Rate 50°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Envalior Arnitel® EM400 TPC-ET, Injection Molding or Extrusion Grade
Envalior Arnitel® EL250 TPC-ET, Injection Molding
Envalior Arnitel® EL550 TPC-ET, Injection Molding
Envalior Arnitel® EL630 TPC-ET, Injection Molding

PDSM8112 / 184813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.