Physical Properties | Metric | English | Comments |
---|
Density | 1.40 g/cc @Temperature 23.0 °C | 0.0506 lb/in³ @Temperature 73.4 °F |
Water Absorption | 0.50 % @Temperature 23.0 °C | 0.50 % @Temperature 73.4 °F |
Permeability | 5.0 @Temperature 23.0 °C | 5.0 @Temperature 73.4 °F |
| 12 @Temperature 23.0 °C | 12 @Temperature 73.4 °F |
| 20 @Temperature 23.0 °C | 20 @Temperature 73.4 °F |
| 50 @Temperature 23.0 °C | 50 @Temperature 73.4 °F |
| 180 @Temperature 23.0 °C | 180 @Temperature 73.4 °F |
Linear Mold Shrinkage | 0.010 cm/cm @Time 900 sec | 0.010 in/in @Time 0.250 hour |
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm @Time 900 sec | 0.0030 in/in @Time 0.250 hour |
|
Mechanical Properties | Metric | English | Comments |
---|
Film Tensile Strength at Yield, MD | 210 MPa | 30500 psi |
Film Tensile Strength at Yield, TD | 260 MPa | 37700 psi |
Film Elongation at Break, MD | >= 150 % | >= 150 % |
Film Elongation at Break, TD | 110 % | 110 % |
Modulus of Elasticity | 4.00 GPa @Temperature 23.0 °C | 580 ksi @Temperature 73.4 °F |
| 5.20 GPa @Temperature 23.0 °C | 754 ksi @Temperature 73.4 °F |
Coefficient of Friction, Static | 0.40 | 0.40 |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | >= 1.00e+11 ohm-cm @Temperature 150 °C | >= 1.00e+11 ohm-cm @Temperature 302 °F |
| >= 1.00e+17 ohm-cm @Temperature 23.0 °C | >= 1.00e+17 ohm-cm @Temperature 73.4 °F |
Surface Resistance | >= 1.00e+12 ohm @Temperature 150 °C | >= 1.00e+12 ohm @Temperature 302 °F |
| >= 5.00e+14 ohm @Temperature 23.0 °C | >= 5.00e+14 ohm @Temperature 73.4 °F |
| >= 5.00e+14 ohm @Temperature 23.0 °C | >= 5.00e+14 ohm @Temperature 73.4 °F |
Dielectric Constant | 2.9 @Frequency 2.40e+8 Hz, Temperature 23.0 °C | 2.9 @Frequency 2.40e+8 Hz, Temperature 73.4 °F |
| 2.9 @Frequency 9.30e+9 Hz, Temperature 23.0 °C | 2.9 @Frequency 9.30e+9 Hz, Temperature 73.4 °F |
| 3.2 @Frequency 1e+6 Hz, Temperature 23.0 °C | 3.2 @Frequency 1e+6 Hz, Temperature 73.4 °F |
| 3.3 @Frequency 50 Hz, Temperature 23.0 °C | 3.3 @Frequency 50 Hz, Temperature 73.4 °F |
| 3.3 @Frequency 1000 Hz, Temperature 23.0 °C | 3.3 @Frequency 1000 Hz, Temperature 73.4 °F |
| 3.6 @Frequency 50 Hz, Temperature 150 °C | 3.6 @Frequency 50 Hz, Temperature 302 °F |
Dielectric Strength | 510 kV/mm @Temperature 23.0 °C | 13000 kV/in @Temperature 73.4 °F |
| 200 kV/mm @Frequency 50 Hz, Temperature 150 °C | 5080 kV/in @Frequency 50 Hz, Temperature 302 °F |
| 290 kV/mm @Frequency 50 Hz, Temperature 23.0 °C | 7370 kV/in @Frequency 50 Hz, Temperature 73.4 °F |
Dissipation Factor | 0.0020 @Frequency 50 Hz, Temperature 23.0 °C | 0.0020 @Frequency 50 Hz, Temperature 73.4 °F |
| 0.0048 @Frequency 50 Hz, Temperature 150 °C | 0.0048 @Frequency 50 Hz, Temperature 302 °F |
| 0.0052 @Frequency 1000 Hz, Temperature 23.0 °C | 0.0052 @Frequency 1000 Hz, Temperature 73.4 °F |
| 0.0060 @Frequency 2.40e+8 Hz, Temperature 23.0 °C | 0.0060 @Frequency 2.40e+8 Hz, Temperature 73.4 °F |
| 0.0060 @Frequency 9.30e+9 Hz, Temperature 23.0 °C | 0.0060 @Frequency 9.30e+9 Hz, Temperature 73.4 °F |
| 0.021 @Frequency 1e+6 Hz, Temperature 23.0 °C | 0.021 @Frequency 1e+6 Hz, Temperature 73.4 °F |
|
Optical Properties | Metric | English | Comments |
---|
Haze | 9.0 % | 9.0 % |
|
Descriptive Properties |
---|
Applications | Adhesive films |
| Adhesive tapes |
| Building insulation |
| Carrier film in veneer- and furniture presses |
| Coating |
| Collar stiffeners |
| Decorative films |
| Drum skins |
| Electrical insulation |
| Film for production of cast films |
| Film for production of GRP-products |
| Films for industrial applications |
| Flexible printed circuits |
| Gaskets and gasket inserts |
| Gloss laminations |
| Insulation tapes |
| Laminating |
| Membranes |
| Metallizing |
| Printing |
| Release |
| Reprography |
| Soundproofing and thermal insulation components |
| Stiffening |
| Tape measures |
| Transfer film |
| Transformers and coils |
Conductivity of Aqueous Extract (µS/cm) | 2 |
F5-value (MPa) | 105 |
| 105 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.