MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe impact and fracture toughness characteristics.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 3737Core at 700°F, 1000hr
 3838Core at 300°F, 100hr
 5858Case at 600°F, 1000hr
 6262Case at 300°F, 1000hr
Tensile Strength, Ultimate 1403 MPa203500 psi371°C Test Temp; 843°C Hardening Temp
 1422 MPa206200 psi371°C Test Temp; 927°C Hardening Temp
 1520 MPa220000 psi24°C Test Temp
Tensile Strength, Yield  1250 MPa
@Strain 0.2 %
181000 psi
@Strain 0.2 %
24°C Test Temp; 927°C Hardening Temp
 1265 MPa
@Strain 0.2 %
183500 psi
@Strain 0.2 %
24°C Test Temp; 843°C Hardening Temp
 965 MPa
@Strain 0.2 %,
Temperature 371 °C
140000 psi
@Strain 0.2 %,
Temperature 700 °F
843°C Hardening Temp
 1020 MPa
@Strain 0.2 %,
Temperature 371 °C
148000 psi
@Strain 0.2 %,
Temperature 700 °F
927°C Hardening Temp
Elongation at Break 11.4 %11.4 %24°C Test Temp; 843°C Hardening Temp
 12.5 %12.5 %24°C Test Temp; 927°C Hardening Temp
 17.5 %
@Temperature 371 °C
17.5 %
@Temperature 700 °F
843°C Hardening Temp
 18.2 %
@Temperature 371 °C
18.2 %
@Temperature 700 °F
927°C Hardening Temp
Reduction of Area 43.5 %43.5 %after 843°C Hardening Temp
 54.9 %54.9 %after 927°C Hardening Temp
 53.6 %
@Temperature 371 °C
53.6 %
@Temperature 700 °F
Modulus of Elasticity 210 GPa30500 ksi
 172 GPa
@Temperature 550.0 °C
24900 ksi
@Temperature 1022 °F
Poissons Ratio  0.292
@Temperature 20.0 °C
0.292
@Temperature 68.0 °F
 0.309
@Temperature 550.0 °C
0.309
@Temperature 1022 °F
Shear Modulus  64.1 GPa
@Temperature 538 °C
9300 ksi
@Temperature 1000 °F
 81.70 GPa
@Temperature 20.0 °C
11850 ksi
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.7 µm/m-°C
@Temperature 21.0 - 204 °C
7.06 µin/in-°F
@Temperature 69.8 - 399 °F
0.20%C
 12.8 µm/m-°C
@Temperature 21.0 - 427 °C
7.11 µin/in-°F
@Temperature 69.8 - 801 °F
0.20%C
Specific Heat Capacity  0.494 J/g-°C
@Temperature 20.0 °C
0.118 BTU/lb-°F
@Temperature 68.0 °F
 0.695 J/g-°C
@Temperature 550.0 °C
0.166 BTU/lb-°F
@Temperature 1022 °F
Thermal Conductivity  33.9 W/m-K
@Temperature 550.0 °C
235 BTU-in/hr-ft²-°F
@Temperature 1022 °F
 48.6 W/m-K
@Temperature 20.0 °C
337 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 316 °C600 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 729 °C1340 °FCase Ac1 Critical Temperaure Ar3
 729 °C1340 °FCore Ac1 Critical Temperaure Ar3
 802 °C1480 °FCase Ac3 Critical Temperaure Ar3
 885 °C1630 °FCore Ac3 Critical Temperaure Ar3
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.060 %0.060 %
Carbon, C 0.19 %0.19 %
Chromium, Cr 1.45 %1.45 %
Iron, Fe 95.6 %95.6 %
Manganese, Mn 0.60 %0.60 %
Molybdenum, Mo 1.0 %1.0 %
Silicon, Si 1.1 %1.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type P20 Mold Steel (UNS T51620)
ASTM A182, Grade F11, Class 2
CBS-600 Carburizing Bearing and Gear Steel
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel

NTIMK006 / 19354

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.