MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ter Hell Plastic Terez® PA 6 7500 GF 30 Polyamide 6, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Medium viscosity Polyamide 6, 30% glass fiber reinforced, good flowability, good impact resistance and bright natural color.

Application: For molding parts with good stiffness and good impact resistance.

Information provided by Ter Hell Plastic GMBH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccISO 1183
Water Absorption 6.3 %6.3 %ISO 62
Moisture Absorption at Equilibrium 1.9 %1.9 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 180 MPa26100 psidry; ISO 527
Tensile Strength, Yield 180 MPa26100 psidry; ISO 527
Elongation at Break 4.0 %4.0 %dry; ISO 527
Tensile Modulus 9.50 GPa1380 ksidry; ISO 527
Charpy Impact Unnotched 8.50 J/cm²40.4 ft-lb/in²dry; ISO 179
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²dry; ISO 179
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FISO 75
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Test 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 270 °C464 - 518 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ter Hell Plastic Terez® PA/PP 7500 GF 7/1 Polyamide/Polypropylene
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber
Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66
Ter Hell Plastic Terez® PA 6.6 7510 GF 50 Polyamide 66, 50% Glass Fiber
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber

PTERH915 / 120653

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.