MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silicon Brass UNS C87400, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Die, Investment, Permanent Mold, Plaster, and Sand.

Applications: Bearings, gears, impellers, rocker arms, valve stems, clamps.

Classified under: Silicon bronzes and silicon brasses. ASTM B584; formerly ASTM B198-13A

As cast values below are for sand casting. Alloy does not respond to heat treating

Key Words: Silicon Brass, ASTM B584; ASTM B198-13A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³Estimated
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070500 kg
 1001003000 kg
Tensile Strength, Ultimate 379 MPa55000 psias cast
Tensile Strength, Yield 165 MPa23900 psias cast
Elongation at Break 30 %30 %as cast
Tensile Modulus 106 GPa15400 ksi
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000260 ohm-cm0.0000260 ohm-cm6.7% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.6 µm/m-°C
@Temperature 20.0 - 300 °C
10.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 2.31 W/m-K16.0 BTU-in/hr-ft²-°F
Melting Point 821 - 916 °C1510 - 1680 °F
Solidus 821 °C1510 °F
Liquidus 916 °C1680 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 83 %83 %
Silicon, Si 3.0 %3.0 %
Zinc, Zn 14 %14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tombasil, UNS C87500, Copper Casting Alloy
Leaded High-Strength Yellow Brass, UNS C86400, Copper Casting Alloy
Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy
Everdur, UNS C87300, Copper Casting Alloy
Silicon Yellow Brass, UNS C87900, Copper Casting Alloy

MC87400b1 / 11920

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.