MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AlphaGary Garaflex™ E 4777-A6 LCF Vinyl Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable
105°C rated low gloss flexible cord jacket compound

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 79 - 8779 - 87
Tensile Strength 17.2 MPa2500 psi
Elongation at Break 350 %350 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -46.0 °C-50.8 °F
Oxygen Index 25 %25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary Garaflex™ G 7766-A4 Thermoplastic Elastomer
AlphaGary Garaflex™ G 7765-A5R Thermoplastic Elastomer
AlphaGary Garaflex™ E 89-086 C3 NF LCF-R Vinyl Thermoplastic Elastomer
AlphaGary Garaflex™ E 4832 Natural UV LCF Vinyl Thermoplastic Elastomer
AlphaGary Evoprene™ HP 3730 High Performance Thermoplastic Elastomer

PGARY9888 / 140674

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.