System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
3M 465 Adhesive Transfer Tape with 3M Adhesive 400
Categories:
Polymer
;
Adhesive
Material Notes:
3M™ Adhesive Transfer Tapes 463, 465, 9457 and 9665 with 3M™ Adhesive 400 are ideal for bonding together a wide variety of similar and dissimilar materials such as metals, glass, wood, papers, paints, and many plastics.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Thickness
50.8
microns
2.00
mil
Tape Only
102
microns
4.00
mil
Release Liner
Mechanical Properties
Metric
English
Comments
Peel Strength
0.27391
kN/m
1.5625
pli
to Steel; ASTM D3330
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
82.0
°C
180
°F
Long term
121
°C
250
°F
Short term
Processing Properties
Metric
English
Comments
Shelf Life
24.0
Month
24.0
Month
Descriptive Properties
Liner
60# Unbleached Densified Kraft
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
3M 9457 Adhesive Transfer Tape with 3M Adhesive 400
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
3M F-9465PC Adhesive Transfer Tape
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
PMM33173 / 167920
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.