MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aearo E-A-R Specialty Composites Isoloss® VL Polyurethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Isoloss® VL elastomers have an extremely low modulus and good damping performance throughout a useful range of 0°C to 49°C. Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.

Information provided by Aearo E-A-R Specialty Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2424
Tensile Strength at Break 1.77 MPa256 psi
Elongation at Break 900 %900 %
Resilience 2323
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °F
Brittleness Temperature -40.0 °C-40.0 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Abrasion ResistanceGood
Compression Set ResistanceGood to Excellent
Damping T max6 dB
Heat Aging; 100°CExcellent
Tear StrengthExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aearo E-A-R Specialty Composites Isoloss® HD Polyurethane Elastomer
Aearo E-A-R Specialty Composites Isoloss® HDF Polyurethane Elastomer
ATG s.r.l. AU-EU Polyurethane Rubber
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE
BASF Elastollan® S 60 AWH TPUR

PEARC26 / 35314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.