MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC PP 623B Polypropylene Random Co-polymer for Cast Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldability for the sealing layers of CPP film.
Films produced using PP 623B will exhibit:
  • Excellent processability
  • Good weldability
  • High clarity
  • High gloss
.

Typical Applications: PP 623B can be used mainly for cast film food and non-food packaging.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ASTM D785
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus, 1% Secant 950 MPa138000 psiASTM D790A
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °FASTM D648
Vicat Softening Point 132 °C270 °FASTM D1525B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film
Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film
Total PPH 6080 Polypropylene Homopolymer, Cast Film

PSABICZ876 / 133072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.