MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics HH 40 Normal Medium and High Heat and Super Duty Brick
Categories: Ceramic

Material Notes: Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rotary Kiln, Heat Curing and Acid Proof Lining

Industry Focuses: Steel, Sponge, Rolling Mills, Coke Oven, Ferrous Foundries, Non-Ferrous, Cement, Petro Chemical, Mineral Processing, Sugar / Paper Mills and Chemical Plants

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.10 g/cc0.0759 lb/in³
Porosity 25 %25 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 19.6 MPa2840 psiCold Crushing
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1400 °C2550 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 40 %40 %
Fe2O3 2.0 %2.0 %
 
Descriptive Properties
PCE Orton32
Permanent Linear Change-1.0 - 1.0%1400°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sharadaa Ceramics HH HG Normal Medium and High Heat and Super Duty Brick
Oxygen-free Copper (OF), UNS C10200, H55 (15%) temper, tubing
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
Cast Stainless Steel HH, ASTM A297

CSHARA077 / 130240

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.