MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistance.

Features: High temperature performance; Excellent strength and stiffness; Excellent dimensional stability
Typical Applications: Electrical motors; Connectors

Information provided by Bieglo Gmbh for Lavergne Performance Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
0.0040 in/in
@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
0.010 in/in
@Thickness 0.0787 in
ASTM D955
Ash 30 %30 %ASTM D2854
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psi5 mm/min; ASTM D638
Flexural Strength 190 MPa27600 psi1.3 mm/min; ASTM D790
Flexural Modulus 9.80 GPa1420 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.700 J/cm
@Temperature 23.0 °C
1.31 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Middle Barrel Temperature 270 - 275 °C518 - 527 °F
Front Barrel Temperature 275 - 280 °C527 - 536 °F
Nozzle Temperature 275 - 290 °C527 - 554 °F
Melt Temperature 275 - 290 °C527 - 554 °F
Mold Temperature 75.0 - 100 °C167 - 212 °F
Injection Pressure 55.0 - 85.0 MPa7980 - 12300 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Evonik Vestodur® X4877 30% Glass Reinforced PBT
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural
Lavergne VYPET VNT 215 PET - PBT 15% Glass Reinforced Polyester
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced

PLAVER902 / 150629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.