MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman Optifilm™ 300 Enhancer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: In architectural coatings Eastman Optifilm™ enhancer 300 is an efficient, low odor, low toxicity coalescent for latex paints. Its broad compatibility, easy incorporation, and excellent hydrolytic stability allow its use in a wide range of latex types. Appropriate for many architectural applications, it is particularly suited for low odor flat and low sheen wall paints. The low odor performance of Eastman Optifilm™ 300 enhancer was evaluated in statistically designed experiments. The technical tip titled Reduce Dispersion Paint Odour Using Eastman Optifilm™ enhancer 300 below outlines the procedure used and the evaluation results. The use of Eastman Optifilm™ enhancer 300 reduces formulated cost by allowing substantial reductions in associative thickeners. Greater than 25% reduction in associative thickener levels can be obtained without compromising rheology characteristics. For more details see the technical tip, Lower Coatings Costs With Texanol™ Ester Alcohol or Eastman Optifilm™ enhancer 300 below. For industrial bake coatings, Eastman Optifilm™ enhancer 300 is an excellent retarder solvent, and is compatible with a variety of resin systems, making it useful over a wide range of application conditions and substrates. It compared favorably in tests versus a widely used retarder solvent in a polyester coil coating application. The results of this evaluation are discussed in the online technical tip entitled Eastman Retarder Solvent and Eastman Optifilm™ enhancer 300 for Industrial Bake Coatings. With a boiling point of 281°C, (vapor pressure 0.0007 kPa @ 20°C), Eastman Optifilm™ enhancer 300 is not classified as a VOC according to European Union Decopaint Directive 2004/42/EC (commonly referred to as the Decopaint Directive); European Union Solvent Emissions Directive; and the China State Environmental Protection Agency. Due to its low toxicity and non-VOC status, Eastman Optifilm™ enhancer 300 has been awarded Green Label Type II certificate in China by the China Environmental United Certification Co. Ltd. (CEC), a wholly-owned subsidiary of the State Environmental Protection Administration of China (SEPA).

Application/Uses:

  • Coatings - Architectural
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
Key Attributes:
  • Excellent associative thickener efficiency
  • Excellent wet and dry film properties
  • Good solubility and compatibility with wide range of coatings systems
  • Improves film formation over a wide range of temperature and relative humidity conditions
  • Low odor
  • LVP-VOC
  • Non-HAP
  • Non-SARA
  • Not classified as a VOC per China State Environmental Protection Agency
  • Not classified as a VOC per European Union
  • Directive 2004/42/EC
  • Not classified as a VOC per European Union Solvent Emissions Directive
  • REACH compliant
  • Readily biodegradable
  • Recognized by China with "Green Label II" certificate (low toxicity, non-VOC and environmental friendly biodegradable product)

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 - 0.948 g/cc0.0340 - 0.0342 lb/in³
Brookfield Viscosity 9.0 cP9.0 cP
Molecular Weight 286.4 g/mol286.4 g/mol
Vapor Pressure 5.87e-12 bar4.40e-9 torr
Surface Tension 27.56 dynes/cm27.56 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Melting Point -70.0 °C-94.0 °FFreezing Point
Boiling Point 281 °C538 °F
Flash Point 143 °C289 °FCleveland Open Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.431.43
 
Descriptive Properties
AppearanceFree from insoluble matter and haze
ColorPT-Co
Fire Point152°CCleveland Open Cup

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Laurel BioComposite Bio-Res™ 20% Composite in HDPE
Evonik REWOPHAT® EAK 8190 Additive
BYK Necowel FLE 55N Clay Additive

PEATM5156 / 222350

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.