MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® T460A Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).

Uses: Injection Molding, Extrusion.

Availability: Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666ASTM D2240
Tensile Strength, Ultimate 19.6 MPa2840 psiASTM D412
Tensile Strength, Yield 2.16 MPa313 psiat 100% elongation; ASTM D412
 3.92 MPa569 psiat 300% elongation; ASTM D412
Elongation at Break 860 %860 %ASTM D412
Tear Strength 58.8 kN/m336 pliDie C; ASTM D624
Compression Set  10 %
@Temperature 23.0 °C,
Time 79200 sec
10 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 75.0 °C167 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Feed Temperature 165 - 180 °C329 - 356 °F
Nozzle Temperature 175 - 190 °C347 - 374 °F
Mold Temperature 10.0 - 40.0 °C50.0 - 104 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hour
Injection Pressure 8.27 - 13.8 MPa1200 - 2000 psi
Hold Pressure 5.52 - 9.65 MPa800 - 1400 psi
Back Pressure 0.207 - 0.552 MPa30.0 - 80.0 psi
Cycle Time - Injection 35 - 45 sec35 - 45 sec
Screw Speed 160 - 200 rpm160 - 200 rpm
 
Descriptive Properties
Injection Time (s)15-20
Metering Zone170-185°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® T465A Thermoplastic Polyurethane
Lubrizol Estane® T365A Thermoplastic Polyurethane
BASF Elastollan® S 70 A SPF TPUR
Lubrizol Estane® T470A Thermoplastic Polyurethane
Lubrizol Estane® T865A Thermoplastic Polyurethane

PNOVEON534 / 121425

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.