MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ecomass® 4710BI71 Filled Polyurethane, Injection Molding
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - Pellets

Processing Method: Injection Molding
Nontoxic alternative to Lead for weighting, balancing and vibration dampening applications

Information provided by Technical Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.50 g/cc2.50 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 MPa2900 psiASTM D638
Elongation at Break 220 %220 %ASTM D638
Tensile Modulus 0.552 GPa80.0 ksiASTM D638
Flexural Strength 44.1 MPa6400 psiASTM D790
Flexural Modulus 0.169 GPa24.5 ksiASTM D790
Izod Impact, Notched 2.46 J/cm4.60 ft-lb/inASTM D256
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 221 °C400 - 430 °F
Mold Temperature 10.0 - 26.7 °C50.0 - 80.0 °F
Drying Temperature 82.2 °C180 °Fdo not over dry
Dry Time 2 hour2 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend

PECOM919 / 133732

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.