MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

VICTREX™ PEEK 150FC30 Easy Flow
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colour black.

Typical Application Areas: Tribological applications with thin cross sections or long flow lengths for high strength. Excellent wear resistance, very low coefficient of friction, low coefficient of thermal expansion. Chemically resistant to aggressive environments.

Information provided by Victrex.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D792
Water Absorption at Saturation  0.30 %
@Temperature 23.0 °C
0.30 %
@Temperature 73.4 °F
ISO 62-1
 0.45 %
@Temperature 100 °C
0.45 %
@Temperature 212 °F
ISO 62-1
Viscosity 275000 cP
@Temperature 400 °C
275000 cP
@Temperature 752 °F
Melt; ISO 11443
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in380°C nozzle, 180°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in380°C nozzle, 180°C tool; ISO 294-4
Spiral Flow 13.0 cm
@Thickness 1.00 mm
5.12 in
@Thickness 0.0394 in
Mold Temp: 180°C, Melt Temp: 380°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ISO 868
Tensile Strength at Break  35.0 MPa
@Temperature 275 °C
5080 psi
@Temperature 527 °F
ISO 527
 50.0 MPa
@Temperature 225 °C
7250 psi
@Temperature 437 °F
ISO 527
 65.0 MPa
@Temperature 175 °C
9430 psi
@Temperature 347 °F
ISO 527
 100 MPa
@Temperature 125 °C
14500 psi
@Temperature 257 °F
ISO 527
 160 MPa
@Temperature 23.0 °C
23200 psi
@Temperature 73.4 °F
ISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 13.5 GPa1960 ksiISO 527
Flexural Strength  45.0 MPa
@Temperature 275 °C
6530 psi
@Temperature 527 °F
ISO 178
 80.0 MPa
@Temperature 175 °C
11600 psi
@Temperature 347 °F
ISO 178
 160 MPa
@Temperature 125 °C
23200 psi
@Temperature 257 °F
ISO 178
 230 MPa
@Temperature 23.0 °C
33400 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Compressive Strength  45.0 MPa
@Temperature 200 °C
6530 psi
@Temperature 392 °F
ISO 604
 110 MPa
@Temperature 120 °C
16000 psi
@Temperature 248 °F
ISO 604
 170 MPa
@Temperature 23.0 °C
24700 psi
@Temperature 73.4 °F
ISO 604
Izod Impact, Notched (ISO) 5.50 kJ/m²2.62 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²ISO 180/U
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1U
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+051e+051V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  120 µm/m-°C
@Temperature <=143 °C
66.7 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 150 µm/m-°C
@Temperature >=143 °C
83.3 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
CTE, linear, Transverse to Flow  45.0 µm/m-°C
@Temperature <=143 °C
25.0 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 110 µm/m-°C
@Temperature >=143 °C
61.1 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
Thermal Conductivity 0.850 W/m-K5.90 BTU-in/hr-ft²-°FAverage; ISO 22007-4
 1.70 W/m-K11.8 BTU-in/hr-ft²-°FAlong flow; ISO 22007-4
Melting Point 343 °C649 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 315 °C599 °FISO 75A-f
Glass Transition Temp, Tg 143 °C289 °FOnset; ISO 11357
 147 °C297 °FMidpoint; ISO 11357
UL RTI, Mechanical with Impact 180 °C356 °FUL 746B
UL RTI, Mechanical without Impact 240 °C464 °FUL 746B
Oxygen Index 43 %
@Thickness 3.20 mm
43 %
@Thickness 0.126 in
ISO 4289
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 100 °C<= 212 °FHopper Temperature
Rear Barrel Temperature 360 °C680 °F
Middle Barrel Temperature 365 - 370 °C689 - 698 °F
Front Barrel Temperature 375 °C707 °F
Nozzle Temperature 380 °C716 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Dry Time 3.00 - 5.00 hour
@Temperature 120 - 150 °C
3.00 - 5.00 hour
@Temperature 248 - 302 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Gate>2 mm or 0.5 x part thickness
Runner>3.5mmmanifold
 >3mm Die/nozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 150CA30 30% Carbon Fiber Reinforced
VICTREX™ PEEK 450FC30 General Purpose
VICTREX™ PEEK 450G™ General Purpose
VICTREX™ PEEK 150PF Easy Flow
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced

PVICT5 / 71829

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.