MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum H13 Tool Steel, UNS T20813  (discontinued **)
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: An excellent hot work grade with an outstanding combination of shock resistance, red hardness, and abrasion resisting properties. Typical application include die casting dies, hot forging dies, hot press dies, dies holder blocks, hot work punches and plastic molding dies.

Information provided by Allegheny Ludlum

Key Words: AMS 6408, ASTM A681(94), FED QQ-T-570(87), SAE J437(70), SAE J438(70), SAE J467(68), BS 4659 BH13, BS 4659 H13, AFNOR NFA35590 Z40CDV5, DIN 17350(80) GX40CrMoV5-1, UNE 36072/2(75) X40CrMoV5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Based on UNS number
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.37 %0.37 %
Chromium, Cr 5.0 %5.0 %
Iron, Fe 91 %91 %as balance
Molybdenum, Mo 1.35 %1.35 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 1.0 %1.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type H13 Hot Work Tool Steel
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Bohler-Uddeholm SUPERIOR® H13 Hot Work Tool Steel
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel

NLTH13 / 18050

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.