MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 300 HB Polycarbonate (PC), Unreinforced - UL94 HB
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Water Absorption 0.15 %0.15 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm
@Thickness 3.17 mm
0.0060 - 0.0090 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 10 - 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 - 12 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength at Break 58.6 MPa8500 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 2.21 GPa320 ksiASTM D 638
Flexural Strength 93.1 MPa13500 psiASTM D 790
Flexural Modulus 2.34 GPa340 ksiASTM D 790
Izod Impact, Notched 8.01 J/cm
@Thickness 3.17 mm
15.0 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D 257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 15.0 kV/mm380 kV/inShort Term; in oil; ASTM D 149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Dry; ASTM D 150
Arc Resistance 120 sec120 secASTM D 495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D 648
Flammability, UL94 HB
@Thickness 0.7937 mm
HB
@Thickness 0.03125 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 82.2 - 121 °C180 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 4300 S-1000 Polysulfone/Polycarbonate Alloy (PSU/PC), Unfilled - UL94
RTP Company RTP 302 SE Polycarbonate (PC), Glass Fiber - Self Extinguishing - Halogen Free - UL94 V-2
RTP Company RTP 300 Polycarbonate (PC), Unreinforced

PQZWA1129 / 90592

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.