MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss and low haze.

Applications: Extrusion Blowmolding Processes

Information provided by Phillips 66.

Key Words: Exceptional gloss and low haze
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.5 MPa3850 psi(2 in/min); ASTM D638
Elongation at Yield 13.5 %13.5 %ASTM D638
Flexural Modulus, 1% Secant 965 MPa140000 psi0.05 in/min; Procedure A; ASTM D790
Izod Impact, Notched 4.27 J/cm8.00 ft-lb/inMethod A; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ASTM D648
 
Descriptive Properties
processBlow Molding
 Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 COPYLENE® CM010G Polypropylene Impact Copolymer
Dow R792-35RNA Polypropylene Random Copolymer Resin
Phillips 66 COPYLENE® CM015G Polypropylene Impact Copolymer
Phillips 66 COPYLENE® CM020N Polypropylene Impact Copolymer
Phillips 66 COPYLENE® CR027 Polypropylene, Homopolymer, Mini-random, BOPP

PCOPY0055 / 140314

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.